LED headlight (DX18)
Temper | Tensile strength | 0.2% proof stress | Elongation | Young's modulus | Thermal conductivity | Electrical conductivity | Castability | |
---|---|---|---|---|---|---|---|---|
MPa | MPa | % | GPa | W/mK | %IACS | |||
DX17 | T5 | 187 | 110 | 13 | 69 | 185 | 46 | B |
DX19 | T5 | 247 | 119 | 5 | 70 | 156 | 37 | A |
ADC12 | F | 296 | 186 | 2 | 71 | 96 | 21 | A |
* Evaluated using 6 mm plate PDF samples.
* The mechanical properties of ADC12 are quoted from the material database of the Japan Aluminum Association.
* Use this data as reference values.
Heatsink (DX26)
Temper | Tensile strength | 0.2% proof stress | Elongation | Electrical conductivity | |
---|---|---|---|---|---|
MPa | MPa | % | %IACS | ||
DX01 | F | 127 | 57 | 30 | 51 |
DX02 | F | 143 | 64 | 22 | 51 |
DX26 | F | 169 | 68 | 18 | 48 |
99.7%Al | F | 83 | 52 | 40 | 57 |
* Evaluated using 6 mm plate PDF samples.
* Use this data as reference values.